MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm Plexiglas® GS 245 Cast Acrylic  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Description: PLEXIGLAS® GS 245 is a cast acrylic with weather resistance specially developed to meet the high optical requirements of the aviation industry. The material is UV-absorbing and can be supplied in both clear-transparent and transparent colored grades. Typical applications are helicopter canopies, glider canopies, sports plane glazing and ultralights.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183, ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-2/1B/5, ASTM D638
Elongation at Break 5.5 %5.5 %ISO 527-2/1B/5, ASTM D 638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
EN 2155-12, ASTM D696
Maximum Service Temperature, Air 105 °C221 °FISO 71-2Ae, ASTM D648
Vicat Softening Point 115 °C239 °FISO 306-B-50
Flame Spread 35.6 mm/min1.40 in/minFire Rating; ASTM D635
 36.0 mm/min1.42 in/minFire Rating; EN 3844-2
Shrinkage 1.5 %
@Thickness 6.35 mm,
Temperature 160 °C
1.5 %
@Thickness 0.250 in,
Temperature 320 °F
16 min
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ISO 489, ASTM D542
Haze 0.50 %0.50 %Original State; EN 2155-9, ASTM D1003
 1.0 %1.0 %after artificial weathering; EN 2155-9, ASTM D1003
Transmission, Visible 89 %89 %after artificial weathering; ASTM D1003
 91 %91 %Original State; EN 2155-5, ASTM D1003
UV Transmittance <= 1.0 %
@Wavelength 290 - 330 nm
<= 1.0 %
@Wavelength 290 - 330 nm
 
Descriptive Properties
Optical DeviationMax 4 minutesEN 2155-7 (ASTM D637)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® GS 249 Cast Acrylic
Röhm Plexiglas® GS 0F00 (222) Cast Acrylic
Röhm Plexiglas® GS 0F00 (233) Cast Acrylic
Trinseo Plexiglas® V825 Acrylic
Trinseo Plexiglas® V045 Acrylic

PHUK031 / 47165

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.