MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.39 - 1.65 g/cc0.0502 - 0.0596 lb/in³Average value: 1.52 g/cc Grade Count:15
Filler Content 30.0 %30.0 %Average value: 30.0 % Grade Count:10
Linear Mold Shrinkage 0.00200 - 0.00300 cm/cm0.00200 - 0.00300 in/inAverage value: 0.00269 cm/cm Grade Count:8
Linear Mold Shrinkage, Transverse 0.00750 - 0.00900 cm/cm0.00750 - 0.00900 in/inAverage value: 0.00806 cm/cm Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 65.0 - 11965.0 - 119Average value: 84.7 Grade Count:3
Tensile Strength, Ultimate 97.0 - 125 MPa14100 - 18100 psiAverage value: 113 MPa Grade Count:15
Elongation at Break 1.20 - 3.10 %1.20 - 3.10 %Average value: 2.05 % Grade Count:15
Modulus of Elasticity 7.40 - 11.0 GPa1070 - 1600 ksiAverage value: 9.35 GPa Grade Count:15
Flexural Yield Strength 150 - 188 MPa21800 - 27300 psiAverage value: 171 MPa Grade Count:15
Flexural Modulus 6.50 - 10.5 GPa943 - 1520 ksiAverage value: 8.61 GPa Grade Count:15
Izod Impact, Notched 0.750 - 1.50 J/cm1.41 - 2.81 ft-lb/inAverage value: 1.05 J/cm Grade Count:3
 1.10 - 1.10 J/cm
@Temperature -40.0 - -40.0 °C
2.06 - 2.06 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.10 J/cm Grade Count:1
Izod Impact, Unnotched 6.90 - 9.10 J/cm12.9 - 17.0 ft-lb/inAverage value: 7.77 J/cm Grade Count:3
Izod Impact, Notched (ISO) 6.00 - 10.0 kJ/m²2.86 - 4.76 ft-lb/in²Average value: 7.91 kJ/m² Grade Count:11
Charpy Impact Unnotched 2.00 - 5.50 J/cm²9.52 - 26.2 ft-lb/in²Average value: 3.82 J/cm² Grade Count:14
Charpy Impact, Notched 0.600 - 1.00 J/cm²2.86 - 4.76 ft-lb/in²Average value: 0.770 J/cm² Grade Count:15
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm1.00e+15 - 1.00e+16 ohm-cmAverage value: 3.25e+15 ohm-cm Grade Count:4
Surface Resistance 1.00e+15 - 1.00e+16 ohm1.00e+15 - 1.00e+16 ohmAverage value: 5.50e+15 ohm Grade Count:4
Dielectric Constant 3.00 - 3.303.00 - 3.30Average value: 3.11 Grade Count:3
Dielectric Strength 16.1 - 35.0 kV/mm409 - 889 kV/inAverage value: 25.6 kV/mm Grade Count:6
Dissipation Factor 0.00200 - 0.01800.00200 - 0.0180Average value: 0.0101 Grade Count:3
Comparative Tracking Index 440 - 600 V440 - 600 VAverage value: 520 V Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 - 48.0 µm/m-°C3.33 - 26.7 µin/in-°FAverage value: 28.7 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 85.0 - 100 µm/m-°C47.2 - 55.6 µin/in-°FAverage value: 91.7 µm/m-°C Grade Count:3
Melting Point 283 - 285 °C541 - 545 °FAverage value: 284 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 268 - 276 °C514 - 529 °FAverage value: 271 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 221 - 262 °C430 - 504 °FAverage value: 247 °C Grade Count:15
UL RTI, Electrical 150 °C302 °FAverage value: 150 °C Grade Count:4
UL RTI, Mechanical without Impact 140 - 150 °C284 - 302 °FAverage value: 149 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:13
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °FAverage value: 102 °C Grade Count:5
Melt Temperature 295 - 310 °C563 - 590 °FAverage value: 302 °C Grade Count:15
Mold Temperature 80.0 - 175 °C176 - 347 °FAverage value: 112 °C Grade Count:10
Drying Temperature 70.0 - 150 °C158 - 302 °FAverage value: 98.7 °C Grade Count:15
Moisture Content 0.0300 %0.0300 %Average value: 0.0300 % Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
Overview of materials for PCT, 40% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced

O3413 / 78212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.