MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LATI Larton MDT16-02 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.95 g/cc0.107 lb/in³
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
Elongation at Break 0.40 %
@Temperature 23.0 °C
0.40 %
@Temperature 73.4 °F
Tensile Modulus 12.0 GPa
@Temperature 23.0 °C
1740 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 0.600 J/cm²2.86 ft-lb/in²
Charpy Impact, Notched 0.150 J/cm²0.714 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °F
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 310 °C554 - 590 °F
Mold Temperature 130 - 140 °C266 - 284 °F
Drying Temperature 130 - 150 °C
@Time 10800 sec
266 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Wacker Belsil® RG 100 Crosspolymer
Trelleborg S550 Silicone Rubber
Schott ZERODUR® K20 Glass Ceramic
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry

PLATH9659 / 177355

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.