MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shinil Chemical SHINCON PPS-CF, Comp. "Y"-1 LCD Rack
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since both materials cost high, there is a need to design the material with cost effectiveness. Also, the current LCD Rack has a concern of sloughing by CF particulates. SHINIL sloves these problems with the CNT composite of polyphenylene sulfide (PPS), polyether sulfone (PES), PEEK, or polyether imide (PEI) by providing the cost effectiveness combined with enhanced mechanical properties. Especially, the wear resistance (coefficient of friction, coefficient of abrasion) of SHINIL CNT composite was much lower than the current PEEK material, which will provide the material for clean/dust free LCD operation environments.

    Features and Benefits
  • Permanent electro conductivity
  • Improved mechanical properties
  • No particulates and no sloughing
  • Lighter weight
  • Recyclability
  • Low abrasion and friction
  • Improved surface
  • Cost effective

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic 0.289
@Time 3600 sec,
Pressure 1.96 MPa
0.289
@Time 1.00 hour,
Pressure 284 psi
0.2 m/s
 
Descriptive Properties
Abrasion Weight (g)0.0148Wear Tester 0.2m/s; 20kgf/cm2; 1hr
Coefficient of Abrasion (10-3 cm2-sec/kgf-m-hr)1.3494Wear Tester 0.2m/s; 20kgf/cm2; 1hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS)
Murtfeldt Murinit® SP Polyphenylene Sulfide
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers
Techmer ES Plastiblend® PPS 05003
Shinil Chemical SHINCON PPS-CF, Comp. "D" LCD Rack

PSHINL02 / 104004

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.