MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Silicon Yellow Brass, UNS C87900, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Die.

Applications: General purpose die casting alloy having moderate strength.

Classified under: Silicon bronzes and silicon brasses. ASTM B176; formerly ASTM ZS331A

Alloy does not respond to heat treating. Data typical for as-die-cast test bars.

Inactive per the Copper Development Association.

Key Words: Silicon Brass, ASTM B176; ASTM ZS331A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7070Typically
Tensile Strength, Ultimate 485 MPa70300 psi
Tensile Strength, Yield 240 MPa
@Strain 0.2 %
34800 psi
@Strain 0.2 %
Elongation at Break 25 %25 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Machinability 80 %80 %UNS C36000 (free-cutting brass) = 100%
Charpy Impact 68.0 J50.2 ft-lbUnnotched
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000011494 ohm-cm
@Temperature 20.0 °C
0.000011494 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.376 J/g-°C0.0899 BTU/lb-°F
Melting Point 900 - 926 °C1650 - 1700 °F
Solidus 900 °C1650 °F
Liquidus 926 °C1700 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.15 %<= 0.15 %
Antimony, Sb <= 0.050 %<= 0.050 %
Arsenic, As <= 0.050 %<= 0.050 %
Copper, Cu >= 63 %>= 63 %
Iron, Fe <= 0.40 %<= 0.40 %
Lead, Pb <= 0.25 %<= 0.25 %
Manganese, Mn <= 0.15 %<= 0.15 %
Nickel, Ni <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si 0.80 - 1.2 %0.80 - 1.2 %
Sulfur, S <= 0.050 %<= 0.050 %
Tin, Sn <= 0.25 %<= 0.25 %
Zinc, Zn 30 - 36 %30 - 36 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tombasil, UNS C87800, Copper Casting Alloy
Tombasil, UNS C87500, Copper Casting Alloy
Silicon Brass UNS C87400, Copper Casting Alloy
Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy
Everdur, UNS C87300, Copper Casting Alloy

MC87900b1 / 11925

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.