MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis KSR4525 Polypropylene Reactor Elastomer Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural color. KSR4525 has been developed for bumper fascias and exterior trims.

Former trade name for this product was Daplen™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inBorealis Method
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiAt 50 mm/min; ISO 527-2
Tensile Modulus 0.940 GPa136 ksiAt 1 mm/min; ISO 527-2
Flexural Modulus 0.970 GPa141 ksiAt 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²13.3 ft-lb/in²ISO 179/1eA
 0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 125 µm/m-°C
@Temperature 23.0 - 80.0 °C
69.4 µin/in-°F
@Temperature 73.4 - 176 °F
Borealis Method
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-2
Vicat Softening Point 52.0 °C126 °FB (50N); ISO 306
 137 °C279 °FA (10N); ISO 306
Shrinkage 0.15 %
@Temperature 90.0 °C,
Time 7200 sec
0.15 %
@Temperature 194 °F,
Time 2.00 hour
Post Shrinkage; Borealis Method
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °FPolymer Mass Temp
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® R 2002 25% Glass Filled TPUR
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating
Borealis Fibremod™ GD302HP Polypropylene, Glass Fiber Reinforced
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
BASF Elastollan® R 2006 20% Glass Filled TPUR

PBOREA162 / 27469

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.