MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Features

Modified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.04 g/cc0.0737 lb/in³
Linear Mold Shrinkage 0.0032 cm/cm0.0032 in/in
Linear Mold Shrinkage, Transverse 0.0046 cm/cm0.0046 in/in
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 270 °C
10 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.0 MPa3920 psi
Elongation at Break 5.0 %5.0 %
Tensile Modulus 3.85 GPa558 ksi
Flexural Strength 85.0 MPa12300 psi
Flexural Modulus 3.68 GPa534 ksi
Charpy Impact Unnotched  0.600 J/cm²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.100 J/cm²
@Temperature -20.0 °C
0.476 ft-lb/in²
@Temperature -4.00 °F
 0.150 J/cm²
@Temperature 23.0 °C
0.714 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Vicat Softening Point 155 °C311 °FB
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °F
Mold Temperature 40.0 - 50.0 °C104 - 122 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.20 %0.20 %
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gichem GIPLENE DB91 Polypropylene
IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound
RTP Company RTP 102 GB 25  Polypropylene (PP) Glass Fiber 15% - Glass Bead 25%
ExxonMobil PP1055E2 Polypropylene Homopolymer
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural

PPLACO297 / 120921

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.