MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Durethan® DP 2802/30 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-free

Application Examples: mixer insert for blenders, washing machine front panels

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 270 °C
17 g/10 min
@Load 4.76 lb,
Temperature 518 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.0 MPa8120 psi5 mm/min; ISO 527-1,-2
Elongation at Break 13.2 %13.2 %5 mm/min; ISO 527-1,-2
Tensile Modulus 3.90 GPa566 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 90.0 MPa13100 psi2 mm/min; ISO 178-A
Flexural Yield Strength 80.0 MPa
@Strain 3.5 %
11600 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 3.70 GPa537 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 6.5 %6.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
838 kV/in
@Thickness 0.0394 in
IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F10°C/min; ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding
 260 - 270 °C500 - 518 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 100 °C176 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® AKV 25 FN00 000000 Nylon 66 (PA66), 25% Glass Fiber Reinforced, Conditioned
Envalior Durethan® DP 2802/30 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber
Envalior Durethan® AKV 15 FN00 000000 Nylon 66 (PA66), 12% Glass Fiber Reinforced, Dry

PLANW9483 / 208338

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.