System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 40% Glass Fiber Filled
;
Nylon 66, Glass Fiber Filled, Flame Retardant
Material Notes:
Notes:
Flammability: Passes, FMVSS 302
Processing Method:
Injection Molding
Forms:
Pellets FMVSS
Information Provided by Teknor Apex
Key Words:
Polyamide 66
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.50
g/cc
1.50
g/cc
ASTM D792
Linear Mold Shrinkage
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength
200
MPa
29000
psi
ASTM D638
Elongation at Break
2.0 %
2.0 %
ASTM D638
Elongation at Yield
2.0 %
2.0 %
ASTM D638
Flexural Strength
283
MPa
41000
psi
ASTM D790
Flexural Modulus
11.0
GPa
1600
ksi
ASTM D790
Izod Impact, Notched
1.33
J/cm
@Temperature 22.8 °C
2.50
ft-lb/in
@Temperature 73.0 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+18
ohm-cm
1.00e+18
ohm-cm
ASTM D257
Dielectric Strength
16.1
kV/mm
@Thickness 3.00 mm
410
kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index
600
V
600
V
UL 746
Thermal Properties
Metric
English
Comments
Melting Point
257
°C
495
°F
DSC
Deflection Temperature at 1.8 MPa (264 psi)
252
°C
485
°F
Unannealed; ASTM D648
Flammability, UL94
HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
Oxygen Index
25 %
25 %
ASTM D2863
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
241
-
257
°C
465
-
495
°F
Middle Barrel Temperature
257
-
271
°C
495
-
520
°F
Front Barrel Temperature
263
-
279
°C
505
-
535
°F
Nozzle Temperature
263
-
282
°C
505
-
540
°F
Melt Temperature
263
-
282
°C
505
-
540
°F
Processing Temperature
Drying Temperature
79.4
°C
175
°F
Moisture Content
0.20 %
0.20 %
Descriptive Properties
Suggested Regrind, max
25
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned)
AKG Polymers Vision PP PPH BL1302 T20 Polypropylene Compound
Spartech PP5120 Talc Filled Homopolymer
Entec Hypro™ F PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
PTEKNO440 / 128617
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.