MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® Z2320 003 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.850 g/cc0.0307 lb/in³
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.021 cm/cm0.021 in/inISO 2577
Melt Flow 58.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
58.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa
@Load 36.5 kg,
Time 30.0 sec
21800 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ISO 527-2
Elongation at Break 20 %20 %Nominal, 50mm/min; ISO 527-2
Elongation at Yield 7.0 %7.0 %ISO 527-2
Modulus of Elasticity 2.80 GPa406 ksiISO 527-2
Charpy Impact Unnotched  13.0 J/cm²
@Temperature -30.0 °C
61.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 13.0 J/cm²
@Temperature 23.0 °C
61.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 1350 MPa196000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 600 V600 VTest solution B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
DIN 53752
Melting Point 166 °C331 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75-2
Vicat Softening Point 150 °C302 °FISO 306
Decomposition Temperature >= 240 °C>= 464 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature 320 - 340 °C608 - 644 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °FHopper Throat
Zone 1 200 °C392 °FFeed zone
Zone 2 200 °C392 °FCompression
Zone 3 200 °C392 °FMetering-zone
Zone 4 200 °C392 °FNozzle
Melt Temperature 200 °C392 °FOptimal
 190 - 230 °C374 - 446 °FInjection-molding
Mold Temperature 60.0 - 120 °C140 - 248 °FInjection-molding
 90.0 °C194 °FOptimal
Drying Temperature 100 °C212 °F
Dry Time 3 hour3 hour
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed<0.3 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2320 006 POM
BASF Ultraform® S1320 003 POM
BASF Ultraform® S2320 003 POM
BASF Ultraform® H2320 004 POM
Asahi Kasei TENAC™-C HC450 Copolymer Acetal (POM)

PBASG0140 / 131773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.