MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® C 9021 AW POM, Tribological
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Chemical abbreviation according to ISO 1043-1: POM

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Water Absorption at Saturation 0.65 %0.65 %ISO 62
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa8410 psi50mm/min; ISO 527-2/1A
Elongation at Break 20 %20 %
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.60 GPa377 ksi50mm/min; ISO 527-2/1A
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²ISO 179/1eU
 13.0 J/cm²
@Temperature -30.0 °C
61.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2300 MPa334000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 1200 MPa174000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FISO 75-1, -2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 190 - 210 °C374 - 410 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 190 - 200 °C374 - 392 °F
Zone 4 190 - 210 °C374 - 410 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 190 - 210 °C374 - 410 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 2.00 MPa<= 290 psi
Screw Speed  70 rpm
@Diameter 55.0 mm
70 rpm
@Diameter 2.17 in
 100 rpm
@Diameter 40.0 mm
100 rpm
@Diameter 1.57 in
 150 rpm
@Diameter 25.0 mm
150 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 9021 SW POM, Tribological
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
Celanese Hostaform® C 9021 FCT1 POM, Tribological
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding

PHCQ343 / 178798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.