MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTOSINT® 1111 colored Polyamide 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTOSINT 1111 colored is a polyamide 12 powder suitable for all-purpose fluidized bed coating.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.016 g/cc0.03671 lb/in³ISO 1183
Water Absorption 1.9 %
@Temperature 100 °C
1.9 %
@Temperature 212 °F
Immersion; ISO 62
Moisture Absorption 0.500 %0.500 %50% RH; ISO 62
 1.30 %1.30 %96% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ISO 868
Ball Indentation Hardness 90.0 MPa13100 psiH30; ISO 2039-1
Tensile Strength, Yield 43.0 MPa6240 psiISO 527-1
Elongation at Break >= 100 %>= 100 %ISO 527-1
Elongation at Yield 6.0 %6.0 %ISO 527-1
Taber Abrasion, mg/1000 Cycles <= 1.0<= 1.0CSI 7, 500g; ASTM D 1242
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Strength 90.0 kV/mm2290 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 196 µm/m-°C
@Temperature 23.0 - 55.0 °C
109 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Specific Heat Capacity 2.35 J/g-°C0.562 BTU/lb-°FDIN 53765
Thermal Conductivity 0.230 - 0.290 W/m-K1.60 - 2.01 BTU-in/hr-ft²-°FDIN 52612
Melting Point 176 °C349 °FISO 3146
 
Descriptive Properties
Active matterK20/P50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOSINT® 1101 white Polyamide 12
Evonik VESTOSINT® 1111 natural color Polyamide 12
Evonik VESTOSINT® 1121 colored Polyamide 12
Evonik VESTOSINT® 1141 colored Polyamide 12
Evonik VESTOSINT® 1141 gray 9.7200 Polyamide 12

PEVONIL170 / 196374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.