MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 2 RM-D natural (3293) PA 6 + ABS Dry
Categories: Polymer; Thermoplastic; ABS Polymer; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: AKROMID B3 2 RM-D natural (3293) is a nonreinforced, UV-stabilized polyamide 6 with limited moisture absorption and light inherent color. Applications are interior and exterior parts with very high impact strength in the automotive industry.

Additive: UV Stabilizer

Features:

  • Ultra High Impact Resistance
  • Low Moisture Absorption
Uses:
  • Automotive Exterior Parts
  • Automotive Interior Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Moisture Absorption 1.6 %
@Temperature 70.0 °C
1.6 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4
Spiral Flow 55.0 cm21.7 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.0 MPa6820 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 50 %>= 50 %50 [mm/min]; ISO 527-2
Tensile Modulus 2.00 GPa290 ksi1 [mm/min]; ISO 527-2
Flexural Modulus 2.10 GPa305 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FUnannealed; ISO 75/A
Vicat Softening Point 112 °C234 °FISO 306/B50
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Aclo Accutech ABS ABS892EV High Heat Grade
Covestro Bayblend® FR3000 PC/ABS Blend
Elix Polymers Elix™ M203FC ABS Polymer
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic

PAKRO243 / 182830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.