MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ TARFLEN SM-1 PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Non Free-Flowing suspension powder for standard compression molding and compounding.

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 g/cc0.0108 lb/in³
Density 2.15 g/cc0.0777 lb/in³ISO 1183
Particle Size 40 µm40 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 868
Ball Indentation Hardness 34.0 MPa4930 psiISO 2039-1
Tensile Strength, Yield 32.0 MPa4640 psiISO 527
Elongation at Break 400 %400 %ISO 527
Izod Impact, Notched 1.40 J/cm2.62 ft-lb/inISO 180
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.10e+18 ohm-cm1.10e+18 ohm-cmIEC 60093
Surface Resistance 4.50e+17 ohm4.50e+17 ohmIEC 60093
Dielectric Strength 72.0 kV/mm1830 kV/inIEC 60243-1
Dissipation Factor 0.000100.00010IEC 60250
Arc Resistance 420 sec420 secIEC 61621
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 125 µm/m-°C
@Temperature 20.0 °C
69.4 µin/in-°F
@Temperature 68.0 °F
ASTM E 831
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 327 °C621 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 370 °C698 °FMolding
Back Pressure 15.0 - 20.0 MPa2180 - 2900 psiMolding Pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Azoty Tarnow™ TARFLEN SG-1 PTFE
Azoty Tarnow™ TARFLEN SG-2 PTFE
Azoty Tarnow™ TARFLEN SM-B30 PTFE
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
Mitsubishi Novaduran® 5010N6-3X Polybutylene Terephthalate

PZAK073 / 72912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.