MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Description

Polyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Melt Flow 10 - 20 g/10 min10 - 20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength at Break 44.8 MPa6500 psiat max load; ASTM D638
Elongation at Yield 6.0 %6.0 %at max load; ASTM D638
Flexural Modulus 5.86 GPa850 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
Izod Impact, Unnotched 2.14 J/cm4.00 ft-lb/inASTM D256
Gardner Impact 0.678 J0.500 ft-lb
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene, Mineral Reinforced
Covestro Bayblend® FR3050 PC/ABS Blend
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 4020 20% Mineral-Filled Polypropylene

PASHU126 / 25090

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.