MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 16 g/10 min
@Load 2.20 kg,
Temperature 260 °C
16 g/10 min
@Load 4.85 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa
@Thickness 3.17 mm
8990 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 40 %
@Thickness 3.17 mm
40 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 96.0 MPa
@Thickness 3.17 mm
13900 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.57 GPa
@Thickness 3.17 mm
373 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FASTM D648
UL RTI, Electrical 60.0 °C140 °F
UL RTI, Mechanical with Impact 60.0 °C140 °F
UL RTI, Mechanical without Impact 60.0 °C140 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 266 °C450 - 510 °F
Middle Barrel Temperature 246 - 274 °C475 - 525 °F
Front Barrel Temperature 246 - 288 °C475 - 550 °F
Nozzle Temperature 246 - 288 °C475 - 550 °F
Melt Temperature 246 - 288 °C475 - 550 °F
Mold Temperature 57.2 - 85.0 °C135 - 185 °F
Drying Temperature 96.1 °C205 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.9 - 110 MPa10000 - 16000 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Screw Speed 25 - 75 rpm25 - 75 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® PCA-NH1015V Flame Retardant
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Covestro Bayblend® FR3010 HF PC/ABS Blend
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant

PZ9PU43 / 21580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.