MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® E 28 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur E 28 is a polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI).

Properties / Applications: As corrosion-resistant primers, coatings based on Desmodur E 28 polyisocyanate can be formulated to contain zinc as zinc-rich primers that give galvanic protection. To ensure satisfactory intercoat adhesion, recoating intervals must be determined. The high NCO content of Desmodur E 28 also makes it an important curing agent for two-component systems. Desmodur E 28 polyisocyanate is an outstanding material for moisture-curing one-component formulations and is highly recommended to prime and seal porous substrates. Clear formulations of this type are effective dust-binding impregnants as well as sealers for cement and other substrates because they can protect the substrate from chemicals, deicing salt, and mineral oils.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
Solids Content 100 %100 %
Viscosity 5200 - 7600 cP5200 - 7600 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 460 °C860 °FPMCC
 
Descriptive Properties
AppearanceBrown liquid
Content15.5-17.5%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® HL BA Polyurethane
Covestro Desmodur® H Polyurethane
Covestro Desmodur® E 744 Polyurethane
Covestro Desmodur® E 23 A Polyurethane
Covestro Desmodur® E 2200/76 Polyurethane

PCOVEST0339 / 202122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.