MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1161 B (SIS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified:
Kraton D1161 BT - supplied as a porous pellet dusted with talc
Kraton D1161 BSM - supplied as a powder dusted with silica

Region: South America, Europe, Asia Pacific, North America, and Japan

Uses: Kraton D1161 B is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccISO 2781
Bulk Density 0.350 g/cc0.0126 lb/in³ASTM D1895 method B
Volatiles <= 0.30 %<= 0.30 %KM 04
Brookfield Viscosity 1100 cP1100 cP25% Toluene Solution at 25°C; KM 06
Melt Flow 8.5 - 19 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.5 - 19 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.50 %<= 0.50 %BT; ISO 247
 2.5 - 5.0 %2.5 - 5.0 %BSM, See Note 1); ISO 247
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30
@Time 30.0 sec
30
@Time 0.00833 hour
Measured on compression molded slabs; ISO 868
Tensile Strength 28.0 MPa4060 psiMeasured on films cast from a toluene solution; ISO 37
Elongation at Break 1300 %1300 %Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.900 MPa
@Strain 300 %
131 psi
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentAntioxidant0.08-0.21%, primary phenolic antioxidant, KM 08
 Polystyrene13.5-16.5%, KM 03
 Total Extractables<1.0%, KM 05
Coupling Efficiency78-84%KM 01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9864 / 132763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.