MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® TPU 810-3070.1 CF15 TPU, 15% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Base Polymer: Polyurethane, Estertype

Filler/Additive System: 15% Carbon Fiber

Special Features: Electrically conductive, reduced surface resistivity

Market Segment: Automotive, Machinery

Application Area: Various

Typical Applications: Functional components

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55
@Time 15.0 sec
55
@Time 0.00417 hour
ISO 868
Tensile Strength 45.0 MPa6530 psiISO 527
Elongation at Break 20 %20 %ISO 527
Tensile Modulus 0.600 GPa87.0 ksiISO 527
Flexural Strength 20.0 MPa2900 psiISO 178
Flexural Modulus 0.600 GPa87.0 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 50 ohm>= 50 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FISO 75-1/-2
Vicat Softening Point 58.0 °C136 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 220 °C392 - 428 °Fextrusion molding
 210 - 230 °C410 - 446 °FInjection molding
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection molding
Drying Temperature  80.0 - 110 °C
@Time 3600 - 10800 sec
176 - 230 °F
@Time 1.00 - 3.00 hour
in a dry air (desiccant) dryer
 80.0 - 110 °C
@Time 3600 - 10800 sec
176 - 230 °F
@Time 1.00 - 3.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolyurethane, Estertype

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 950 Urethane Thermoplastic Elastomer
PlastiComp Complet® LGF40 - ETPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Mocom (ALBIS) ALCOM® TPU 810/4073 AR10 TPU, 10% Aramid Powder Reinforced
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel

PALBIS8204 / 242263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.