MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aptek DI-STRATE 95211 Microwave/RF Foam Substrate
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset

Material Notes: DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.

Uses: Space Antennas

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³Foam
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040
Compressive Yield Strength 2.69 MPa390 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.5
@Frequency 2.00e+9 Hz
1.5
@Frequency 2.00e+9 Hz
Dissipation Factor 0.0043
@Frequency 2.00e+9 Hz
0.0043
@Frequency 2.00e+9 Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aptek DI-STRATE 95173-1 Microwave/RF Foam Substrate
MarkeTech Resorcinol Formaldehyde Aerogel
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Coastal Enterprises Plus™ PBLT-75 High Density Urethane Foam

PAPTEK51 / 24213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.