MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Park Aerospace Nelcote® E-722 Epoxy Prepreg, 285 Aramid Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.

Key Features and Benefits:

  • Epoxy resin system optimized for use with woven aramid reinforcements
  • Meets requirements of MIL-R-9300B, Type 1
  • Long out-time for easy processing

Applications/Qualifications:

  • Military Helicopters
  • Engine Nacelles
  • Work Platforms
  • Doors
  • Air Frames

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 3.0 %
@Temperature 135 °C
<= 3.0 %
@Temperature 275 °F
8 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 517 MPa
@Temperature 23.9 °C
75000 psi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Tensile Modulus 31.7 GPa
@Temperature 23.9 °C
4600 ksi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Flexural Strength 427 MPa
@Temperature 23.9 °C
62000 psi
@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 28.3 GPa
@Temperature 23.9 °C
4100 ksi
@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 172 MPa
@Temperature 23.9 °C
25000 psi
@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 31.0 GPa
@Temperature 23.9 °C
4500 ksi
@Temperature 75.0 °F
Dry; ASTM D695
Shear Strength 29.0 MPa
@Temperature 23.9 °C
4200 psi
@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
 
Processing PropertiesMetricEnglishComments
Gel Time 1.00 - 6.00 min1.00 - 6.00 min
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Prepreg Resin Content (%)52-58
Resin Flow (%)15-35325°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Park Aerospace Nelcote® E-766B Epoxy Prepreg, 285 Kevlar® Reinforced
Solvay CYCOM® 919 Epoxy Prepreg with Kevlar 49 Aramid Fiber, Weave Style 285
Solvay CYCOM® 950-1 Epoxy Prepreg with 52% 285 Kevlar Fabric

PPARK009 / 89281

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.