System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Film Grade
Material Notes:
EX5 is a high density polyethylene with 1-Butene as co monomer.
Applications: film extrusion, counter bag, carrier bag, wrapping films
Information provided by Iran Petrochemical Commercial Co.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.949
g/cc
0.0343
lb/in³
ISO 1183
Melt Flow
0.28
g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.28
g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
8.0
g/10 min
@Load 21.6 kg,
Temperature 190 °C
8.0
g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
60
60
ISO 868
Tensile Strength at Break
35.0
MPa
5080
psi
ISO 527
Tensile Strength, Yield
24.0
MPa
3480
psi
ISO 527
Film Elongation at Break, MD
<= 400 %
<= 400 %
ISO 527
Film Elongation at Break, TD
<= 450 %
<= 450 %
ISO 527
Elmendorf Tear Strength MD
20.4
g
20.4
g
ISO 6383-2
Elmendorf Tear Strength TD
45.9
g
45.9
g
ISO 6383-2
Dart Drop Test
220
g
0.485
lb
ASTM D1709
Film Tensile Strength at Break, MD
<=
45.0
MPa
<=
6530
psi
ISO 527
Film Tensile Strength at Break, TD
<=
40.0
MPa
<=
5800
psi
ISO 527
Thermal Properties
Metric
English
Comments
Softening Point
75.0
°C
167
°F
ISO 306
Brittleness Temperature
>=
-80.0
°C
>=
-112
°F
ASTM D746-72
Processing Properties
Metric
English
Comments
Melt Temperature
200
-
230
°C
392
-
446
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene
Iran Petrochemical (PCC) 7000F High Density Polyethylene
PIPC203 / 149665
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.