MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 5216 Epoxy - Woven Aramid Fiber Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 5216 is a 200 – 250°F (93 – 121°C) curing, modified epoxy resin. Service temperature range is -67 to 180°F (-55 to 82°C). This prepreg is manufactured by hot melt processing and is virtually solvent-free. Typical applications include rotorblade spars and skins. Aramid reinforced CYCOM 5216 has application in helicopter structure, rotorblades and high impact resistant laminates. Available in unidirectional, woven and, on special order, roving forms; also with carbon and glass fiber.

Features & Benefits:

  • Excellent fatigue resistance
  • High flow with long shop life
  • Autoclave and press cure
  • Maximum continuous service temperature up to 180°F (82°C)
  • Low pressure moldable
  • Good tack and drape characteristics
  • Excellent translation of fiber strength
  • Tape laying machine capable
Applications:
  • Aircraft secondary structure
  • Rotorcraft structure and blade applications
Mechanical property data for Standard Cure, Aramid Fiber, Woven (Kevlar style 285) tested in warp direction.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.235 g/cc0.04462 lb/in³Cured, Neat Resin
Volatiles <= 0.50 %
@Time 900 sec
<= 0.50 %
@Time 0.250 hour
QC-PT-16
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 524 MPa76000 psiASTM D638
Elongation at Break 1.35 %1.35 %ASTM D638
Tensile Modulus 30.0 GPa4350 ksiASTM D638
Compressive Strength 255 MPa37000 psiASTM D695
Compressive Modulus 26.0 GPa3770 ksiASTM D695
Shear Strength 38.6 MPa5600 psiShort Beam; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 88.0 °C190 °FWet
 
Processing PropertiesMetricEnglishComments
Processing Temperature 93.3 - 121 °C200 - 250 °FCure Temp.
Gel Time 4.00 - 6.00 min
@Temperature 135 °C
4.00 - 6.00 min
@Temperature 275 °F
Neat Resin
Shelf Life  >= 1.00 Month
@Temperature 22.0 °C
>= 1.00 Month
@Temperature 71.6 °F
 3.00 Month
@Temperature 4.00 °C
3.00 Month
@Temperature 39.2 °F
sealed container
 6.00 Month
@Temperature -18.0 °C
6.00 Month
@Temperature -0.400 °F
sealed container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 5216 Epoxy - Unidirectional S-Glass Prepreg
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy
Solvay CYCOM® E773 and E773FR Epoxy Neat Resin
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Graphite Fabric and 195FAW Epoxy

PCYTED097 / 180399

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.