MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 200 TC-C-21 FR Nylon 6/6 (PA); Thermally Conductive - Electrically Conductive - Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %ASTM D 638
Tensile Modulus 17.2 GPa2500 ksiASTM D 638
Flexural Strength 96.5 MPa14000 psiASTM D 790
Flexural Modulus 13.8 GPa2000 ksiASTM D 790
Izod Impact, Notched 0.267 J/cm
@Thickness 3.20 mm
0.500 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 2.14 J/cm
@Thickness 3.20 mm
4.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.30 W/m-K9.03 BTU-in/hr-ft²-°FThrough-plane; ASTM E 1530
 4.003 W/m-K27.78 BTU-in/hr-ft²-°FIn-plane; ASTM E 1461-92
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C530 - 570 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 399 X 91042 Polycarbonate (PC), Thermally Conductive - Electrically Insulative
RTP Company RTP 399 X 95997 B Polycarbonate (PC), Thermally Conductive - Electrically Conductive
RTP Company RTP 4099 X 128640 Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive - Preliminary Datasheet
RTP Company RTP 1399 X 130032 A Polyphenylene Sulfide (PPS); Thermally Conductive - Glass Fiber - Electrically Conductive - EMI/RFI Shielding - (Preliminary Data Sheet)
RTP Company RTP 1399 X 128638 Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Insulative

PQZUA21583 / 134794

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.