MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal KLINGER® top-chem-2000 PTFE Gasketing
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Fire Tested - API6FA
  • Universal application use in the chemical and petrochemical industries
  • FDA compatible
  • Ideal for higher temperatures and pressures
  • Holds shape for thermal cycles
Permits/Certifications: BAM certification; KTW proposal; DIN-DVGW permit; Fire Tested API6FA; FDA conformity; TA-Luft certification; Germanischer Lloyd; United States Coast Guard; Registro Italiano Navale; Det Norske Veritas AS and RoHS Certificate 2002/95/EG

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.50 g/cc0.0903 lb/in³
Thickness 1500 microns59.1 milThickness tested
 
Descriptive Properties
Compressibility2 percentASTM F36
Klinger Cold/Hot Compression2 percent75°F/7,250 psi
 5 percent480°F/7,250 psi
Sealability0.05 mg/smDIN 28090-2
 0.5 ml/minDIN 3535/6
Stress Relaxation28 MPaDIN 52913, 16h 4,350 psi, 300°F
 35 MPaDIN 52913, 16h 7,250 psi, 570°F
Thickness/Weight Increase1/1%H2SO4, 100%: 18h/75°F
 1/2%HNO3, 100%: 18h/75°F
 1/3%NaOH, 33%: 72h/230°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
G-10 Fiberglass Epoxy Laminate Sheet
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800)
Syensqo (Solvay Specialty Polymers) Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
Saint-Gobain Chemfab® 6 Primary PTFE-Coated Glass

PTHERM901 / 146054

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.