MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.47 - 1.62 g/cc0.0531 - 0.0585 lb/in³Average value: 1.51 g/cc Grade Count:25
Filler Content 15.0 - 20.0 %15.0 - 20.0 %Average value: 18.3 % Grade Count:15
Water Absorption 0.180 - 1.60 %0.180 - 1.60 %Average value: 0.520 % Grade Count:18
Moisture Absorption at Equilibrium 0.300 - 0.600 %0.300 - 0.600 %Average value: 0.500 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00800 cm/cm0.00100 - 0.00800 in/inAverage value: 0.00334 cm/cm Grade Count:25
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm0.00250 - 0.00900 in/inAverage value: 0.00599 cm/cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 98.0 - 12598.0 - 125Average value: 118 Grade Count:13
Tensile Strength, Ultimate 81.4 - 150 MPa11800 - 21800 psiAverage value: 117 MPa Grade Count:22
 80.0 - 110 MPa
@Temperature 60.0 - 150 °C
11600 - 16000 psi
@Temperature 140 - 302 °F
Average value: 95.0 MPa Grade Count:1
Tensile Strength, Yield 124 - 133 MPa18000 - 19300 psiAverage value: 129 MPa Grade Count:4
Elongation at Break 1.50 - 5.00 %1.50 - 5.00 %Average value: 2.97 % Grade Count:25
 2.60 - 3.00 %
@Temperature 60.0 - 150 °C
2.60 - 3.00 %
@Temperature 140 - 302 °F
Average value: 2.78 % Grade Count:1
Elongation at Yield 2.50 - 2.50 %
@Temperature 150 - 150 °C
2.50 - 2.50 %
@Temperature 302 - 302 °F
Average value: 2.50 % Grade Count:1
Modulus of Elasticity 4.48 - 13.8 GPa650 - 2000 ksiAverage value: 6.63 GPa Grade Count:22
 5.90 - 6.50 GPa
@Temperature 60.0 - 150 °C
856 - 943 ksi
@Temperature 140 - 302 °F
Average value: 6.21 GPa Grade Count:1
Flexural Yield Strength 138 - 193 MPa20000 - 28000 psiAverage value: 175 MPa Grade Count:20
Flexural Modulus 3.79 - 6.89 GPa550 - 1000 ksiAverage value: 5.72 GPa Grade Count:20
Compressive Yield Strength 124 - 138 MPa18000 - 20000 psiAverage value: 131 MPa Grade Count:8
Shear Modulus 0.200 - 1.00 GPa
@Temperature 50.0 - 225 °C
29.0 - 145 ksi
@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Izod Impact, Notched 0.320 - 0.854 J/cm0.600 - 1.60 ft-lb/inAverage value: 0.664 J/cm Grade Count:20
Izod Impact, Unnotched 1.87 - 7.47 J/cm3.50 - 14.0 ft-lb/inAverage value: 5.99 J/cm Grade Count:16
Izod Impact, Notched (ISO) 6.00 - 6.50 kJ/m²2.86 - 3.09 ft-lb/in²Average value: 6.33 kJ/m² Grade Count:3
 6.50 - 6.50 kJ/m²
@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 - 4.70 J/cm²11.9 - 22.4 ft-lb/in²Average value: 3.85 J/cm² Grade Count:4
 4.50 - 4.50 J/cm²
@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.400 - 0.650 J/cm²1.90 - 3.09 ft-lb/in²Average value: 0.575 J/cm² Grade Count:4
 0.650 - 0.650 J/cm²
@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.650 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 200 - 1.00e+17 ohm-cm200 - 1.00e+17 ohm-cmAverage value: 1.01e+16 ohm-cm Grade Count:20
Surface Resistance 200 - 1.00e+14 ohm200 - 1.00e+14 ohmAverage value: 6.67e+13 ohm Grade Count:3
Dielectric Constant 3.80 - 4.203.80 - 4.20Average value: 3.92 Grade Count:9
Dielectric Strength 14.8 - 37.0 kV/mm375 - 940 kV/inAverage value: 17.9 kV/mm Grade Count:13
Dissipation Factor 0.00200 - 0.01000.00200 - 0.0100Average value: 0.00680 Grade Count:9
Arc Resistance 70.0 - 80.0 sec70.0 - 80.0 secAverage value: 71.3 sec Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 39.6 µm/m-°C11.1 - 22.0 µin/in-°FAverage value: 32.6 µm/m-°C Grade Count:13
 23.0 - 23.0 µm/m-°C
@Temperature 140 - 180 °C
12.8 - 12.8 µin/in-°F
@Temperature 284 - 356 °F
Average value: 23.0 µm/m-°C Grade Count:2
Thermal Conductivity 0.190 - 0.303 W/m-K1.32 - 2.10 BTU-in/hr-ft²-°FAverage value: 0.281 W/m-K Grade Count:8
Maximum Service Temperature, Air 180 - 220 °C356 - 428 °FAverage value: 201 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 210 - 224 °C410 - 435 °FAverage value: 217 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 204 - 220 °C399 - 428 °FAverage value: 211 °C Grade Count:24
Glass Transition Temp, Tg 225 °C437 °FAverage value: 225 °C Grade Count:3
Flammability, UL94 V-0V-0Grade Count:21
Oxygen Index 39.0 - 44.5 %39.0 - 44.5 %Average value: 41.5 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 366 °C176 - 690 °FAverage value: 320 °C Grade Count:8
Melt Temperature 343 - 390 °C650 - 734 °FAverage value: 363 °C Grade Count:14
Mold Temperature 93.0 - 190 °C199 - 374 °FAverage value: 156 °C Grade Count:21
Drying Temperature 135 - 180 °C275 - 356 °FAverage value: 150 °C Grade Count:13
Moisture Content 0.0400 %0.0400 %Average value: 0.0400 % Grade Count:9
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:9
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
BASF Ultrason® E 3010 PES
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled

O3712 / 78240

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.