MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Applications & Industries:
General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is a good bearing material on soft metals & in high speed contact.
Chemical: Dynamic & shaft seals; Construction; Bridge bearings; and Slide bearings. Engineering: Anti - friction bearing cages & bearing plates; Bearings, bushes, shaft bearings / seals (in combustion engines); Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology: Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.

CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, some fluorine compounds & halogen gases at elevated temperatures.

Information provided by Dalau

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 - 2.18 g/cc0.0759 - 0.0788 lb/in³BS2782:Pt6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 6765 - 67ASTM D2240
Tensile Strength 13.5 - 25.0 MPa1960 - 3630 psiMolding Direction; BS2782:Pt3
Elongation at Break 120 - 250 %120 - 250 %Molding Direction; BS2782:Pt3
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmASTM D257
Surface Resistance 1.00e+12 ohm1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.780 W/m-K5.41 BTU-in/hr-ft²-°FMolding Direction; ASTM C177
Melting Point 327 °C621 °FASTM D3417
Maximum Service Temperature, Air 260 °C500 °F
 300 °C572 °FShort Periods
Minimum Service Temperature, Air -200 °C-328 °F
Flash Point 630 °C1170 °FASTM D1929
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Dalau Dalcon 001 100% Virgin PTFE
Dalau Dalcon 086 100% Virgin PTFE modified polymer

PDALAU003 / 132991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.