MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is transparent. It is tough and resistant to stress whitening. It has fast forming cycles and is easy to form. Eastar PCTG Copolyester 5445 is sterilizable by both gamma radiation and ethylene oxide (ETO) methods. Its scrap can be reused.

Applications/Uses

  • Bags
  • Credit cards
  • Gaming cards
  • Identification cards
  • Plastic Cards
  • Rigid medical
  • Blister packaging
  • Debit cards
  • Gift cards
  • Phone cards
  • Rapid deployment flood walls
  • Smart cards
  • Key Attributes

  • Excellent clarity
  • Effective barrier properties
  • Excellent colorability
  • Good stiffness
  • Sterilizable with ethylene oxide, electron beam, and gamma rays
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.23 g/cc0.0444 lb/in³ASTM D1505
    Melt Density 1.08 g/cc
    @Temperature 285 °C
    0.0390 lb/in³
    @Temperature 545 °F
    ASTM D1238
    Water Vapor Transmission 7.00 g/m²/day0.451 g/100 in²/dayASTM F372
    Oxygen Transmission 11.0 cc-mm/m²-24hr-atm27.9 cc-mil/100 in²-24hr-atmASTM D3985
    Carbon Dioxide Transmission 49.0 cc-mm/m²-24hr-atm124 cc-mil/100 in²-24hr-atmASTM D1434
    Thickness 250 microns9.84 milASTM D374
     
    Mechanical PropertiesMetricEnglishComments
    Film Tensile Strength at Yield, MD 45.0 MPa6530 psiASTM D882
    Film Tensile Strength at Yield, TD 44.0 MPa6380 psiASTM D882
    Tensile Modulus 1.60 GPa232 ksiTD; ASTM D882
     1.60 GPa232 ksiMD; ASTM D882
    Coefficient of Friction 0.500.50ASTM D1894
    Elmendorf Tear Strength, MD >= 12.0 g/micron>= 305 g/milASTM D1922
    Elmendorf Tear Strength, TD >= 12.0 g/micron>= 305 g/milASTM D1922
    Dart Drop 1.84 g/micron46.7 g/mil23°C; ASTM D1709
     2.16 g/micron54.9 g/milat -18°C; ASTM D1709
    Film Tensile Strength at Break, MD 57.0 MPa8270 psiASTM D882
    Film Tensile Strength at Break, TD 53.0 MPa7690 psiASTM D882
     
    Thermal PropertiesMetricEnglishComments
    Specific Heat Capacity  1.09 J/g-°C
    @Temperature 10.0 °C
    0.261 BTU/lb-°F
    @Temperature 50.0 °F
    DSC
     1.14 J/g-°C
    @Temperature 30.0 °C
    0.272 BTU/lb-°F
    @Temperature 86.0 °F
    DSC
     1.64 J/g-°C
    @Temperature 100 °C
    0.392 BTU/lb-°F
    @Temperature 212 °F
    DSC
     1.86 J/g-°C
    @Temperature 180 °C
    0.445 BTU/lb-°F
    @Temperature 356 °F
    DSC
     2.16 J/g-°C
    @Temperature 290 °C
    0.516 BTU/lb-°F
    @Temperature 554 °F
    DSC
    Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FASTM C177
    Glass Transition Temp, Tg 87.0 °C189 °FASTM D1525
     
    Optical PropertiesMetricEnglishComments
    Refractive Index 1.56
    @Wavelength 589.3 nm
    1.56
    @Wavelength 589.3 nm
    nD; ASTM D542
    Haze 1.0 %1.0 %ASTM D1003
    Gloss 98 %98 %at 60°; ASTM D2457
    Transmission, Visible 91 %91 %Total Transmittance; ASTM D1003

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Eastman Eastar DN011 Copolyester
    Eastman Eastar DN004 PCTG Copolyester
    Eastman DuraStar DS1000 Polymer, Natural
    Eastman Eastar 5445 PCTG Copolyester, Injection Molded
    Eastman Eastar DN001 PCTG Copolyester

    PE9058 / 35114

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.