MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chi Mei Wonderlite® PC-110 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Medium Viscosity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa14500 psiH358/30; ISO 2039-1
Tensile Strength at Break 75.0 MPa10900 psi50 mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ISO 527
Elongation at Break 120 %120 %50 mm/min; ISO 527
Flexural Strength 90.0 MPa13100 psi2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 80.0 kJ/m²38.1 ft-lb/in²ISO 180/4A
Charpy Impact, Notched 7.50 J/cm²35.7 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °Fannealed; ISO 75
 143 °C289 °Funannealed; ISO 75
Vicat Softening Point  145 °C
@Load 5.00 kg
293 °F
@Load 11.0 lb
50°C/hr; ISO 306
 150 °C
@Load 1.00 kg
302 °F
@Load 2.20 lb
50°C/hr; ISO 306
Flammability, UL94 V-2
@Thickness 2.54 mm
V-2
@Thickness 0.100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 70G30L NC010 PA66-GF30
Chi Mei Wonderlite® PC-115 Polycarbonate
Chi Mei Wonderlite® PC-110U Polycarbonate - UV Stabilized
Chi Mei Wonderlite® PC-122 Polycarbonate
Chi Mei Wonderlite® PC-110V Polycarbonate - Flame Retardant

PCHI953 / 109441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.