MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mercury Telluride, HgTe (Coloradoite)
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Key Words: Chalcogenide; Semiconductor; Tellurium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.17 g/cc0.295 lb/in³
a Lattice Constant 6.4623 Å6.4623 Å
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 300300N/mm²
 
Electrical PropertiesMetricEnglishComments
Band Gap -0.0600 eV-0.0600 eV
Electron Mobility, cm²/V-s 2500025000
Hole Mobility, cm²/V-s 350350
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.60 µm/m-°C
@Temperature 20.0 °C
2.56 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.164 J/g-°C0.0392 BTU/lb-°F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Melting Point 670 °C1240 °F
Heat of Formation 242 kJ/mol242 kJ/mol
Debye Temperature -31.0 °C-23.8 °F
 
Descriptive Properties
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mercury Selenide, HgSe (Tiemannite)
Assab Steels 705M Machinery Steel
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer
Indium Arsenide, InAs
Indium Phosphide, InP

DSEN24 / 3037

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.