MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

21Cr-32Ni-Ti-Al IRON BASED 21Cr-32Ni-Ti-Al SUPERALLOY FOR CORROSION AND HEAT-RESISTING PLATE (NCF 800H-P)
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes:

Creep and rupture data provided by NIMS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  6.00 - 8.00 MPa
@Temperature 950 °C,
Time 3.60e+8 sec
870 - 1160 psi
@Temperature 1740 °F,
Time 100000 hour
 9.00 - 12.0 MPa
@Temperature 900 °C,
Time 3.60e+8 sec
1310 - 1740 psi
@Temperature 1650 °F,
Time 100000 hour
 13.0 - 20.0 MPa
@Temperature 850 °C,
Time 3.60e+8 sec
1890 - 2900 psi
@Temperature 1560 °F,
Time 100000 hour
 22.0 - 29.0 MPa
@Temperature 800 °C,
Time 3.60e+8 sec
3190 - 4210 psi
@Temperature 1470 °F,
Time 100000 hour
 35.0 - 43.0 MPa
@Temperature 750 °C,
Time 3.60e+8 sec
5080 - 6240 psi
@Temperature 1380 °F,
Time 100000 hour
 54.0 - 62.0 MPa
@Temperature 700 °C,
Time 3.60e+8 sec
7830 - 8990 psi
@Temperature 1290 °F,
Time 100000 hour
 84.0 - 94.0 MPa
@Temperature 650 °C,
Time 3.60e+8 sec
12200 - 13600 psi
@Temperature 1200 °F,
Time 100000 hour
 130 - 148 MPa
@Temperature 600 °C,
Time 3.60e+8 sec
18900 - 21500 psi
@Temperature 1110 °F,
Time 100000 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
21Cr-32Ni-Ti-Al IRON BASED 21Cr-32Ni-Ti-Al ALLOY FOR HEAT EXCHANGER SEAMLESS TUBES (NCF 800H TB)
Moso Bamboo
Guadua Bamboo
Borosilicate Glass
Aluminum 6061-T6; 6061-T651

NIMS028 / 77545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.