MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 70G33L BK031 PA66-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 33% Glass Reinforced Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³DAM; ISO 1183
Water Absorption 5.7 %
@Thickness 2.00 mm
5.7 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.80 %
@Thickness 2.00 mm
1.80 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psi50% RH; ISO 527-1/-2
 200 MPa29000 psiDAM; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %DAM; ISO 527-1/-2
 4.0 %4.0 %50% RH; ISO 527-1/-2
Tensile Modulus 8.00 GPa1160 ksi50% RH; ISO 527-1/-2
 11.0 GPa1600 ksiDAM; ISO 527-1/-2
Flexural Modulus 9.30 GPa1350 ksiDAM; ISO 178
Poissons Ratio 0.340.3450% RH
 0.340.34DAM
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -40.0 °C
4.28 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 83.0 µm/m-°C46.1 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °C502 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 252 °C486 °FDAM; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
DAM; IEC 60695-11-10
Flame Spread 35.0 mm/min
@Thickness 1.00 mm
1.38 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 305 °C545 - 581 °FRange, Injection
 295 °C563 °FOptimum, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)10VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,GF33,M1CGR,S14-110
Max. screw tangential speed (m/s)0.2Injection
Odor Class3VDA 270
Part Marking Code>PA66-GF33<ISO 11469
PolymerPA66-GF33
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA66-GF33ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 70G33L NC010 PA66-GF33
Celanese Celcon® GB25 POM, 25% Glass Reinforced
Celanese Celcon® GB10 POM, 10% Glass Reinforced
Celanese Celcon® LW90FS-K POM, Tribological
Celanese Zytel® 70G33HS1L BK031 PA66-GF33

PDSX5331 / 197971

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.