System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ravago Manufacturing Americas Hylex P1317L Polycarbonate
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
Polycarbonate, High Flow, UV-stabilized version, DAM
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
ISO 1183
Water Absorption
0.15 %
0.15 %
24 hr, Immersed; ISO 62
Melt Flow
17
g/10 min
@Load 1.20 kg,
Temperature 300 °C
17
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
72
72
ISO 2039
Tensile Strength at Break
70.0
MPa
10200
psi
ISO 527-1
Elongation at Break
115 %
115 %
ISO 527-1
Flexural Strength
93.0
MPa
13500
psi
ISO 178
Flexural Modulus
2.38
GPa
345
ksi
ISO 178
Izod Impact, Notched (ISO)
54.0
kJ/m²
25.7
ft-lb/in²
ISO 180
Electrical Properties
Metric
English
Comments
Volume Resistivity
4.00e+16
ohm-cm
4.00e+16
ohm-cm
ASTM D257
Dielectric Strength
16.1
kV/mm
410
kV/in
ASTM D149
Arc Resistance
120
sec
120
sec
ASTM D495
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
140
°C
284
°F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi)
129
°C
264
°F
ISO 75-2/A
Shrinkage, MD
0.50 - 0.70 %
@Thickness 3.17 mm
0.50 - 0.70 %
@Thickness 0.125 in
ISO 294-4
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Entec Hylex® P1017FR Polycarbonate
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
Covestro Makroblend® UT305 PC/PET Blend
Ravago Manufacturing Americas Hylex P2010G20 Polycarbonate, 20% Glass Fiber, General Purpose, DAM
Ravago Manufacturing Americas Hylex P1325L Polycarbonate
PRAVAGO3205 / 222176
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.