MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

H.C. Starck MoCu 70/30 Molybdenum-Copper Composite Material
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A thermal conductivity over 200 W/m K is producible.

Range of Application: Switching contacts for high-voltage and medium-voltage, heat sinks for passive thermal management, electrodes for erosive processing.

Information provided by H.C. Starck.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.60 - 10.0 g/cc0.347 - 0.361 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130 - 170
@Load 62.5 kg
130 - 170
@Load 138 lb
2.5 mm ball
Tensile Strength, Ultimate >= 290 MPa>= 42100 psi
Modulus of Elasticity 210 GPa30500 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000038 ohm-cm0.0000038 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.20 µm/m-°C
@Temperature 20.0 - 100 °C
4.56 µin/in-°F
@Temperature 68.0 - 212 °F
 8.60 µm/m-°C
@Temperature 20.0 - 300 °C
4.78 µin/in-°F
@Temperature 68.0 - 572 °F
 8.80 µm/m-°C
@Temperature 20.0 - 450 °C
4.89 µin/in-°F
@Temperature 68.0 - 842 °F
Thermal Conductivity >= 190 W/m-K>= 1320 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 27 - 33 %27 - 33 %
Molybdenum, Mo 67 - 73 %67 - 73 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T4; 6061-T451
Aluminum 6061-T6; 6061-T651
Oxygen-free Electronic Copper (OFE), UNS C10100, H00 Temper, flat products
Aluminum 3003-O
Aluminum 6061-O

NHCST957 / 130846

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.