MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics AN-985 Aluminum Nitride
Categories: Ceramic; Nitride; Oxide; Aluminum Oxide

Material Notes: Excellent thermal conductivity and good electrical properties. Used for heat sinks and substrates in electronics industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.30 g/cc0.119 lb/in³Fired
Porosity 0.00 %0.00 %Apparent, fully dense
Particle Size 7.0 µm7.0 µmGrain size
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 310 GPa
@Temperature 20.0 °C
45000 ksi
@Temperature 68.0 °F
Flexural Strength 285 MPa
@Temperature 20.0 °C
41300 psi
@Temperature 68.0 °F
3-point
Poissons Ratio 0.210.21
Shear Modulus 128 GPa18600 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm
@Temperature 20.0 °C
>= 1.00e+13 ohm-cm
@Temperature 68.0 °F
Dielectric Constant 8.8
@Frequency 100000 Hz
8.8
@Frequency 100000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.60 µm/m-°C
@Temperature 20.0 - 400 °C
2.00 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity 175 W/m-K
@Temperature 20.0 °C
1210 BTU-in/hr-ft²-°F
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
Sapco Aluminum Nitride
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride
CeramTec Alunit® Aluminum Nitride

CMORG51 / 90429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.