MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, Thermal Postcure
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Description: Somos® ProtoTherm 12120 stereolithography material is the perfect solution for applications requiring resistance to heat and humidity. Somos® ProtoTherm 12120 excels at producing highly detailed, extremely accurate parts. The material is dimensionally stable when exposed to heat and humidity making it a good candidate for high temperature fluid flow analysis, functional prototypes, and limited run, non-critical end-use parts such as wiring harnesses and support connectors in electronic devices.

Key Benefits:

  • Extremely Precise Accuracy for Small Details
  • Resistant to Heat up to 250°F (121°C)
  • Stable in High Humidity Environments
Ideal Applications:
  • High-Temperature Fluid Flow Analysis
  • Functional Prototypes Requiring Heat and Humidity Resistance
  • High-Detail Parts
  • Low Volume Connectors and Harnesses for Electronics

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Industry leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including Stereolithography printing technology. Free 3D quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc
@Temperature 25.0 °C
0.0415 lb/in³
@Temperature 77.0 °F
Water Absorption 0.24 %0.24 %ASTM D570-98
Viscosity 550 cP
@Temperature 30.0 °C
550 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ASTM D2240
Tensile Strength, Yield 77.0 MPa11200 psiASTM D638M
Elongation at Break 4.5 %4.5 %ASTM D638M
Modulus of Elasticity 3.25 GPa471 ksiASTM D638M
Flexural Strength 103 MPa14900 psiASTM D790M
Flexural Modulus 3.06 GPa444 ksiASTM D790M
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.53
@Frequency 1e+6 Hz
3.53
@Frequency 1e+6 Hz
ASTM D150-98
 3.84
@Frequency 1000 Hz
3.84
@Frequency 1000 Hz
ASTM D150-98
 3.89
@Frequency 60.0 Hz
3.89
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 16.4 kV/mm417 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear  56.7 µm/m-°C
@Temperature -40.0 - 0.000 °C
31.5 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-00
 66.3 µm/m-°C
@Temperature 0.000 - 50.0 °C
36.8 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-00
 92.7 µm/m-°C
@Temperature 50.0 - 100 °C
51.5 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-00
 158.7 µm/m-°C
@Temperature 100 - 150 °C
88.17 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 126.2 °C259.2 °FASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 110.7 °C231.3 °FASTM D648-98c
Glass Transition Temp, Tg 111 °C232 °FASTM E1545-00
 
Descriptive Properties
AppearanceRed
Dp (mm)6Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)63Exposure that gives 0.254mm thickness
Ec (mJ/cm2)11.8Critical exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, Thermal Postcure
DSM Somos® WaterShed® 11120 Water-resistant resin for stereolithography
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure

PDSMT020 / 93540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.