MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Data provided by Adell Plastics, Inc.

Key Words: Polyamide 66; Nylon 6,6; Adell Plastics, Inc.; Adell Nylon 6/6; Polyamide 6/6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ASTM D792
Water Absorption 0.60 %0.60 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9898ASTM D785
Hardness, Rockwell R 122122ASTM D785
Tensile Strength, Ultimate 138 MPa20000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
Flexural Modulus 7.60 GPa1100 ksiASTM D790
Compressive Yield Strength 255 MPa37000 psiASTM D695
Izod Impact, Notched 0.300 J/cm0.562 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 249 °C480 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 246 °C475 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding
Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Domo Technyl® A 216 V40 40% Glass Filled Nylon 66

PDEL64 / 29625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.