MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan PU Corporation UR80 Polyester Urethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: UR80 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of conventional rubber manufacturing equipment and techniques to yield finished urethane parts.

Compounds of urethane rubber can be molded by compression, injection, and transfer molding procedures. Excellent mold definition is obtainable in press cures. The linear shrinkage of vulcanizates of UR varies somewhat with the type of loading, but, in general this value is approximately 1.5%, which is comparable to that of neoprene.

Excellent mold release is provided by lubricant of M-7 or silicone mold release lubricants, but indiscriminate use can cause poor flow and knitting problems.

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Mooney Viscosity 35 - 65
@Temperature 100 °C
35 - 65
@Temperature 212 °F
ML 1-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Tensile Strength at Break 12.6 MPa1830 psi
Elongation at Break 420 %420 %
300% Modulus 9.65 MPa
@Strain 300 %
1400 psi
@Strain 300 %
Tear Strength 47.3 kN/m270 pliDie C
Compression Set 96 %
@Temperature 158 °C,
Time 79200 sec
96 %
@Temperature 316 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Processing Temperature 152 - 171 °C305 - 340 °F
Cure Time 5.00 - 45.0 min0.0833 - 0.750 hour
 
Descriptive Properties
ColorWhite to cream
Health HazardNone
OdorFaint, characteristic
Physical FormSolid
Storage StabilityExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Taiwan PU Corporation UR50 Polyester Urethane Rubber
3M Scotchkote™ 80XRG 539 Urethane Elastomer
SK Chemicals SKYTHANE® 180A R series Polyurethane
Taiwan PU Corporation UR70 Polyester Urethane Rubber
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound

PTPU48 / 70904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.