MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestoran® 1100 nf PPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Filler-free, amorphous PPE resin.

Applications: Automobile industry, household and laboratory equipment, washing machines, dishwashers.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Melt Flow 46 g/10 min46 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi
Elongation at Break 20 %20 %
Elongation at Yield 4.0 %4.0 %
Modulus of Elasticity 2.20 GPa319 ksi
Charpy Impact Unnotched 11.5 J/cm²54.7 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
Tensile Impact Strength 42.0 kJ/m²20.0 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 3.00e+14 ohm3.00e+14 ohm
Dielectric Constant  2.0
@Frequency 100 Hz
2.0
@Frequency 100 Hz
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dielectric Strength 41.0 kV/mm1040 kV/in
Dissipation Factor  0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
 0.00090
@Frequency 100 Hz
0.00090
@Frequency 100 Hz
Comparative Tracking Index 400 V400 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °F
Vicat Softening Point 116 °C241 °F50°C/hr/50 N

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled
BASF Luranyl® KR 2456/3 Polyphenylene Ether + Styrene-Butadiene Blend
Evonik Vestoran® 1900 PPE Compound
Mitsubishi Iupiace® EHM1010A m-Polyphenylene Ether (m-PPE)
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate

PHUM48 / 47481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.