MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CIMBAR FlexTalc® 610D Ultrafine Talc for TPO Applications, Densified
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprietary process that results in talc products which have very high aspect ratios, are easily dispersed, provide heat aging and offer compounded color. They are available in powder and densified (D) forms.

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.78 g/cc2.78 g/cc
Bulk Density 0.689 g/cc0.0249 lb/in³Loose
Brightness 66 %66 %wet
 96 %96 %Hunter Rd, dry
Oil Absorption 68 %68 %g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.50 %0.50 %
Loss On Ignition 7.5 %7.5 %
Particle Size 1.0 µm1.0 µmD50
 <= 5.5 µm<= 5.5 µmPSD 98%
pH 8.78.7
 
Component Elements PropertiesMetricEnglishComments
Al2O3 <= 1.0 %<= 1.0 %
CaO <= 1.0 %<= 1.0 %
Fe2O3 <= 1.0 %<= 1.0 %
MgO 30 %30 %
SiO2 60 %60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CIMBAR FlexTalc® 1222D Ultrafine Talc for TPO Applications, Densified
CIMBAR NANO-FLEX® Talc - D for TPO Applications
CIMBAR FlexTalc® 610 Ultrafine Talc for TPO Applications
CIMBAR FlexTalc® 815D Ultrafine Talc for TPO Applications, Densified
CIMBAR FlexTalc® 815 Ultrafine Talc for TPO Applications

CIMBAR926 / 133408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.