MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Engineered Syntactic Systems SF-25 Subsea Macrosphere Syntactic Void Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: The four part SF-25 kit was developed specifically to meet the critical needs of void space filling at operating pressures to 1000 psi. This system utilizes carbon fiber reinforced epoxy macrospheres in combination with the standard microsphere syntactic to provide low density lling, yielding a greater than 60% increase in buoyancy per cubic foot. In this system, cavities are pre-filled with the ~ 0.625 inch diameter macrospheres, specially fabricated to withstand the operating hydrostatic pressure of the vessel. The liquid syntactic is then injected into the cavities around the macrospheres and allowed to cure at room temperature. The resultant low-density system will provide an average of 39 pounds of buoyancy per cubic foot of void space.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.400 g/cc<= 0.0145 lb/in³
Water Absorption <= 3.0 %
@Time 86400 sec
<= 3.0 %
@Time 24.0 hour
at 2272 ft.depth
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 17.2 MPa>= 2500 psi
Compressive Modulus >= 0.827 GPa>= 120 ksi
Hydrostatic Design Basis 27.6 MPa4000 psiHydrostatic Crush Strength (9090 feet)
 
Descriptive Properties
ColorWhite/Tan
Service Depth (feet)2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg AEM Syntac® 351 Syntactic Foam
Trelleborg AEM Eccofloat® DS-39/11500 Syntactic Foam
Trelleborg AEM Eccofloat® DS-35/8130 Syntactic Foam
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres
Trelleborg AEM Eccofloat® TG-39/10000 Syntactic Foam

PESS965 / 93187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.