MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX™ WG102 Polyaryletherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Unreinforced

Material Notes: Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliant
WG102 does not contain polyetrafluoroethylene (PTFE) or other halogenated additives

Typical Application Areas: Higher temperature tribological applications for high strength and stiffness. Excellent wear resistance, low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.

Information Provided by Victrex.

Key Words: PAEK
Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³Crystalline; ISO 1183
Viscosity 575000 cP
@Temperature 400 °C
575000 cP
@Temperature 752 °F
Melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/in410°C nozzle, 190°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/in410°C nozzle, 190°C tool; ISO 294-4
Spiral Flow  36.0 cm
@Thickness 3.00 mm
14.2 in
@Thickness 0.118 in
Mold Temp: 190°C, Melt Temp: 415°C; Victrex
 85.0 cm
@Thickness 1.00 mm
33.5 in
@Thickness 0.0394 in
Mold Temp: 190°C, Melt Temp: 415°C; Victrex
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ISO 868
Tensile Strength at Break  55.0 MPa
@Temperature 275 °C
7980 psi
@Temperature 527 °F
ISO 527
 85.0 MPa
@Temperature 175 °C
12300 psi
@Temperature 347 °F
ISO 527
 130 MPa
@Temperature 125 °C
18900 psi
@Temperature 257 °F
ISO 527
 195 MPa
@Temperature 23.0 °C
28300 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 19.5 GPa2830 ksiISO 527
Flexural Strength  75.0 MPa
@Temperature 275 °C
10900 psi
@Temperature 527 °F
ISO 178
 145 MPa
@Temperature 175 °C
21000 psi
@Temperature 347 °F
ISO 178
 220 MPa
@Temperature 125 °C
31900 psi
@Temperature 257 °F
ISO 178
 290 MPa
@Temperature 23.0 °C
42100 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Compressive Strength  55.0 MPa
@Temperature 250 °C
7980 psi
@Temperature 482 °F
ISO 604
 80.0 MPa
@Temperature 200 °C
11600 psi
@Temperature 392 °F
ISO 604
 175 MPa
@Temperature 120 °C
25400 psi
@Temperature 248 °F
ISO 604
 250 MPa
@Temperature 23.0 °C
36300 psi
@Temperature 73.4 °F
ISO 604
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²19.0 ft-lb/in²ISO 180/U
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eA
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cm1V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  9.00 µm/m-°C
@Temperature <=143 °C
5.00 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 10.0 µm/m-°C
@Temperature >=143 °C
5.56 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
CTE, linear, Transverse to Flow  35.0 µm/m-°C
@Temperature <=143 °C
19.4 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 90.0 µm/m-°C
@Temperature >=143 °C
50.0 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
Thermal Conductivity 1.30 W/m-K9.02 BTU-in/hr-ft²-°FAverage; ISO/CD 22007-4
 2.20 W/m-K15.3 BTU-in/hr-ft²-°FAlong flow; ISO 22007-4
Melting Point 373 °C703 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 367 °C693 °FISO 75-f
Glass Transition Temp, Tg 152 °C306 °FOnset; ISO 11357
 180 °C356 °FMidpoint; ISO 11357
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 100 °C<= 212 °FHopper Temperature
Rear Barrel Temperature 390 °C734 °F
Middle Barrel Temperature 395 - 400 °C743 - 752 °F
Front Barrel Temperature 405 °C761 °F
Nozzle Temperature 410 °C770 °F
Mold Temperature 190 - 215 °C374 - 419 °F
Drying Temperature 120 - 150 °C248 - 302 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour
 
Descriptive Properties
ColorBlack
Gate> 2mm or 0.5 x part thickness
RunnerDie/nozzle > 3mm, manifold > 3.5mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ WG101 Polyaryletherketone
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
VICTREX™ PEEK 150FC30 Easy Flow
Avient Trilliant™ HC HC6200-5001 XR Grey High Denisty Polyamide 12 (Nylon 12)
Victrex APTIV™ 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled

PVICTB11 / 122199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.