MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also a PPA resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³DAM; ISO 1183
Filler Content 35 %35 %DAM
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 215 MPa
@Temperature 23.0 °C
31200 psi
@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.3 %
@Temperature 23.0 °C
2.3 %
@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 11.5 GPa
@Temperature 23.0 °C
1670 ksi
@Temperature 73.4 °F
DAM; ISO 527
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 264 °C507 °FDAM; ISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 325 °C617 °FDAM; Optimum
 320 - 330 °C608 - 626 °FDAM
Mold Temperature 150 °C302 °FDAM; optimum
 140 - 160 °C284 - 320 °FDAM
Drying Temperature 100 °C212 °FDAM
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourDAM
Moisture Content <= 0.10 %<= 0.10 %DAM
 
Descriptive Properties
AppearanceBlack ColorDAM
FillerGlass ReinforcedDAM
FormsPelletsDAM
GenericPolyphthalamide (PPA)DAM
Material StatusPreliminary DataDAM
Part Marking Code>PA6T/XT-GF35<ISO 11469; DAM
 >PPA-GF35<SAE J1344; DAM
Processing MethodInjection MoldingDAM
Product CategoryGlass Reinforced ResinsDAM
Region Available - GlobalYesDAM
Resin IdentificationPA6T/XT-IGF35ISO 1043; DAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Celanese Zytel® HTN 51G50HSL BK083 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 54G35HSLR BKB336 Polyphthalamide (PPA)

PZDSZ1420 / 140237

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.