MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen PP H2150 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Hostalen PP H2150 is a natural, nucleated polypropylene homopolymer. The product is typically used in the applications pipes, extruded and compression molded sheets. The material Hostalen PP H2150 is not intended for medical and pharmaceutical applications. Applications: General Sheet Extrusion, Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow  0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 1.5 g/10 min
@Load 5.00 kg,
Temperature 230 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psiISO 527-1,-2
Elongation at Yield 11 %11 %ISO 527-1,-2
Tensile Modulus 1.50 GPa218 ksiISO 527-1,-2
Charpy Impact, Notched  0.430 J/cm²
@Temperature 0.000 °C
2.05 ft-lb/in²
@Temperature 32.0 °F
ISO 179
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 95.0 °C203 °FB50; ISO 306
 158 °C316 °FA50; ISO 306
DSC Induction Temperature 160 °C320 °FISO 3146
 
Descriptive Properties
Processing Methodcompression molding, pipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® 5000 V/2 Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5000 /V2-EP Self Extinguishing Polypropylene, Flame Resistant
LyondellBasell Hostacom PP HH42L 356015 Polypropylene
LyondellBasell Hostalen PP H2142 12 Polypropylene Copolymer
LyondellBasell Hostalen PP H2450 Polypropylene

PEQT8507 / 220142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.