MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 - 1.00 g/cc0.0330 - 0.0361 lb/in³Average value: 0.952 g/cc Grade Count:216
Water Absorption 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:15
Viscosity  270000 - 2.10e+6 cP
@Temperature 190 - 190 °C
270000 - 2.10e+6 cP
@Temperature 374 - 374 °F
Average value: 1.26e+6 cP Grade Count:7
 270000 - 2.10e+6 cP
@Shear Rate 100 - 1000 1/s
270000 - 2.10e+6 cP
@Shear Rate 100 - 1000 1/s
Average value: 1.26e+6 cP Grade Count:7
Environmental Stress Crack Resistance 10.0 - 10000 hour10.0 - 10000 hourAverage value: 2940 hour Grade Count:61
 15.5 - 15.5 hour
@Temperature 50.0 - 100 °C
15.5 - 15.5 hour
@Temperature 122 - 212 °F
Average value: 1290 hour Grade Count:18
 >= 5.00 hour
@Temperature 80.0 - 80.0 °C
>= 5.00 hour
@Temperature 176 - 176 °F
Average value: 1290 hour Grade Count:2
 >= 5.00 hour
@Pressure 0.920 - 0.920 MPa
>= 5.00 hour
@Pressure 133 - 133 psi
Average value: 1290 hour Grade Count:2
 530 - 530 hour
@Temperature 50.0 - 100 °C
530 - 530 hour
@Temperature 122 - 212 °F
Average value: 1290 hour Grade Count:8
 530 - 530 hour
@Thickness 1.90 - 2.00 mm
530 - 530 hour
@Thickness 0.0748 - 0.0787 in
Average value: 1290 hour Grade Count:8
Oxidative Induction Time (OIT) 10.0 - 45.0 min10.0 - 45.0 minAverage value: 23.5 min Grade Count:29
 20.0 - 120 min
@Temperature 200 - 220 °C
20.0 - 120 min
@Temperature 392 - 428 °F
Average value: 47.4 min Grade Count:43
Thickness 6350 - 119000 microns250 - 4700 milAverage value: 44900 microns Grade Count:14
Melt Flow 0.0290 - 47.0 g/10 min0.0290 - 47.0 g/10 minAverage value: 4.63 g/10 min Grade Count:210
Base Resin Melt Index  0.400 - 0.400 g/10 min
@Temperature 190 - 190 °C
0.400 - 0.400 g/10 min
@Temperature 374 - 374 °F
Average value: 0.400 g/10 min Grade Count:1
 0.400 - 0.400 g/10 min
@Load 5.00 - 5.00 kg
0.400 - 0.400 g/10 min
@Load 11.0 - 11.0 lb
Average value: 0.400 g/10 min Grade Count:1
Ash 1.00 - 2.02 %1.00 - 2.02 %Average value: 1.55 % Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 54.0 - 71.054.0 - 71.0Average value: 63.5 Grade Count:119
Ball Indentation Hardness 40.0 - 55.0 MPa5800 - 7980 psiAverage value: 49.6 MPa Grade Count:7
Tensile Strength, Ultimate 18.0 - 40.7 MPa2610 - 5900 psiAverage value: 32.5 MPa Grade Count:77
Tensile Strength, Yield 16.5 - 31.7 MPa2390 - 4600 psiAverage value: 23.8 MPa Grade Count:185
Elongation at Break 195 - 1550 %195 - 1550 %Average value: 696 % Grade Count:170
Elongation at Yield 7.00 - 600 %7.00 - 600 %Average value: 19.9 % Grade Count:57
Modulus of Elasticity 0.700 - 1.34 GPa102 - 195 ksiAverage value: 1.06 GPa Grade Count:46
Flexural Modulus 0.300 - 1.65 GPa43.5 - 240 ksiAverage value: 0.961 GPa Grade Count:135
Secant Modulus 0.500 - 1.34 GPa72.5 - 194 ksiAverage value: 0.974 GPa Grade Count:18
Izod Impact, Notched 0.785 - 9.19 J/cm1.47 - 17.2 ft-lb/inAverage value: 4.17 J/cm Grade Count:58
 0.490332 - 3.43233 J/cm
@Temperature -20.0 - 0.000 °C
0.918594 - 6.43016 ft-lb/in
@Temperature -4.00 - 32.0 °F
Average value: 1.91 J/cm Grade Count:9
Izod Impact, Unnotched 1.10 - 1.10 J/cm
@Temperature 220 - 220 °C
2.06 - 2.06 ft-lb/in
@Temperature 428 - 428 °F
Average value: 1.10 J/cm Grade Count:1
Izod Impact, Notched (ISO) 0.490 - 24.0 kJ/m²0.233 - 11.4 ft-lb/in²Average value: 15.9 kJ/m² Grade Count:17
Charpy Impact, Notched 0.500 J/cm² - NB2.38 ft-lb/in² - NBAverage value: 2.05 J/cm² Grade Count:16
 0.300 - 1.60 J/cm²
@Temperature -30.0 - 0.000 °C
1.43 - 7.61 ft-lb/in²
@Temperature -22.0 - 32.0 °F
Average value: 1.15 J/cm² Grade Count:10
Tensile Impact 64.1 - 148 J/cm120 - 277 ft-lb/inAverage value: 120 J/cm Grade Count:3
Coefficient of Friction 0.2000.200Average value: 0.200 Grade Count:14
Coefficient of Friction, Static 0.2000.200Average value: 0.200 Grade Count:14
Tensile Creep Modulus, 1 hour 640 - 850 MPa92800 - 123000 psiAverage value: 783 MPa Grade Count:7
Tensile Creep Modulus, 1000 hours 300 - 360 MPa43500 - 52200 psiAverage value: 344 MPa Grade Count:8
Hydrostatic Design Basis 5.50 - 11.0 MPa798 - 1600 psiAverage value: 10.4 MPa Grade Count:34
 6.89476 - 6.90 MPa
@Temperature 60.0 - 60.0 °C
1000.00 - 1000 psi
@Temperature 140 - 140 °F
Average value: 6.90 MPa Grade Count:22
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1e+05 - 1.00e+17 ohm-cm1e+05 - 1.00e+17 ohm-cmAverage value: 2.80e+16 ohm-cm Grade Count:6
Surface Resistance 10000 - 1.00e+16 ohm10000 - 1.00e+16 ohmAverage value: 8.00e+15 ohm Grade Count:5
Dielectric Constant 2.35 - 2.452.35 - 2.45Average value: 2.38 Grade Count:5
Dielectric Strength 16.0 - 18.0 kV/mm406 - 457 kV/inAverage value: 16.6 kV/mm Grade Count:5
Dissipation Factor 0.000200 - 0.02000.000200 - 0.0200Average value: 0.00683 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 216 µm/m-°C66.7 - 120 µin/in-°FAverage value: 173 µm/m-°C Grade Count:32
 90.0 - 500 µm/m-°C
@Temperature -20.0 - 100 °C
50.0 - 278 µin/in-°F
@Temperature -4.00 - 212 °F
Average value: 295 µm/m-°C Grade Count:1
Specific Heat Capacity 2.00 - 2.10 J/g-°C0.478 - 0.502 BTU/lb-°FAverage value: 2.01 J/g-°C Grade Count:9
 2.60 - 2.60 J/g-°C
@Temperature 150 - 150 °C
0.621 - 0.621 BTU/lb-°F
@Temperature 302 - 302 °F
Average value: 2.60 J/g-°C Grade Count:8
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FAverage value: 0.400 W/m-K Grade Count:7
 0.200 - 0.200 W/m-K
@Temperature 150 - 150 °C
1.39 - 1.39 BTU-in/hr-ft²-°F
@Temperature 302 - 302 °F
Average value: 0.200 W/m-K Grade Count:8
Melting Point 53.9 - 138 °C129 - 280 °FAverage value: 126 °C Grade Count:54
Maximum Service Temperature, Air 72.8 - 264 °C163 - 507 °FAverage value: 120 °C Grade Count:21
Deflection Temperature at 0.46 MPa (66 psi) 57.0 - 99.0 °C135 - 210 °FAverage value: 73.1 °C Grade Count:33
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C118 °FAverage value: 47.8 °C Grade Count:14
Vicat Softening Point 67.0 - 132 °C153 - 270 °FAverage value: 116 °C Grade Count:90
Brittleness Temperature -118 - 70.0 °C-180 - 158 °FAverage value: -78.6 °C Grade Count:75
DSC Induction Temperature 129 - 260 °C264 - 500 °FAverage value: 170 °C Grade Count:12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 210 °C374 - 410 °FAverage value: 200 °C Grade Count:5
Die Temperature 200 - 210 °C392 - 410 °FAverage value: 205 °C Grade Count:7
Melt Temperature 136 - 260 °C277 - 500 °FAverage value: 205 °C Grade Count:17
Head Temperature 200 - 210 °C392 - 410 °FAverage value: 205 °C Grade Count:6
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.00 - 2.50 %2.00 - 2.50 %Average value: 2.30 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
Overview of materials for High Density Polyethylene (HDPE), Impact Grade

O4005 / 78280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.