MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, or mineral filled polypropylene.

Examples: Compatibilising short-and long glass fibres and PP applications such as automotive applications (instrument panel carrier, front-end, door modules, etc.) and Wood filled polymer composites.

Mode of action and advantages: PRIEX® 20097 is a polypropylene, grafted with a very high content of maleic anhydride. The grafted maleic anhydride introduces polarity to the polymer achieving compatibility between polyolefins and more polar polymers like EVOH.

Advantages: Excellent mechanical properties, good cost / performance; Ultra low smell, low VOC and emissions; Excellent wetting properties as a result of very low viscosity (hyperfluid grade); Excellent coupling agent for shortand long glass filled polyolefins providing enhanced physical, mechanical and thermal properties; Excellent coupling agent for natural fibre reinforced polymer composites or wood flour reinforced polymer composites; Free flowing pellets; and Safe and easy handling.

Food contact: PRIEX® 20097 composition meets the requirements of Commission Directive 2002/72/EC and further amendments.

Former Addcomp product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxidative Induction Time (OIT) 25 min
@Temperature 190 °C
25 min
@Temperature 374 °F
ISO 11357-6
Melt Flow 25 - 30 g/10 min
@Load 1.20 kg,
Temperature 190 °C
25 - 30 g/10 min
@Load 2.65 lb,
Temperature 374 °F
die 8/1; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.8 MPa3600 psiISO 527-2
Elongation at Break 1.55 %1.55 %ISO 527-2
Modulus of Elasticity 1.70 GPa247 ksi1 mm/min; ISO 527-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 164 °C320 - 327 °FISO 11357-3
Crystallization Temperature 113 - 115 °C235 - 239 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 116.3 °C241.3 °FISO 75
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 280 °C<= 536 °F
 
Descriptive Properties
AppearanceWhite or slightly yellow granules
Free Aleic Anhydride<50 mg/kgSolvay method
Grafted Maleic Anhydride0.45%Solvay method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 25050 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 25097 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 25093 Maleic Anhydride Grafted PP random copolymer
ArcelorMittal 04 High formability steel for drawing, Cold rolled

PPADDC04 / 130316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.