MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7000 Series Copper Roofing Granule (Little Rock)
Categories: Ceramic

Material Notes: 3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treated to promote adhesion to asphalt. These copper containing granules are part of a system that is used to control algae.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.44 - 1.54 g/cc0.0520 - 0.0556 lb/in³
Density 2.55 - 2.70 g/cc0.0921 - 0.0975 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.0 - 7.06.0 - 7.0
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %
 
Descriptive Properties
AppearanceVarious shades of Black, Gray, Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Rock Elm Wood
Sodium Chloride, NaCl (Halite)
Overview of materials for Medium Alloy Steel
Overview of materials for Cast Stainless Steel
Lubriplate Rock Drill Oil Specialty Oil 10R and Fluid

PMM35431 / 170178

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.