MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Quartzel® Fused Quartz Textiles
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is available in the form of yarn, roving, chopped strands, wool, and felts.

It is used in dielectric applications (radomes, circuit boards), thermal applications (high temp insulation for aerospace, asbestos replacement, furnace linings, hot gas filtration), and reinforcement for composites (with resins such as phenolics or epoxies).

Information provided by Saint-Gobain Quartz PLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 7.07.0
Tensile Strength, Ultimate 6000 MPa870000 psiVirgin Filament
Elongation at Break 7.7 %7.7 %Virgin Filament
Modulus of Elasticity 78.0 GPa11300 ksiVirgin Filament
Poissons Ratio 0.160.16
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 6.00e+10 ohm-cm
@Temperature 800 °C
6.00e+10 ohm-cm
@Temperature 1470 °F
Dielectric Constant 3.74
@Frequency 1e+9 Hz
3.74
@Frequency 1e+9 Hz
Dielectric Strength 37.0 kV/mm940 kV/in
Dissipation Factor 0.00020
@Frequency 1e+9 Hz
0.00020
@Frequency 1e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.540 µm/m-°C
@Temperature 20.0 °C
0.300 µin/in-°F
@Temperature 68.0 °F
isotropic (axial vs. radial)
Specific Heat Capacity 0.750 J/g-°C0.179 BTU/lb-°F
Thermal Conductivity 1.38 W/m-K9.58 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1050 °C1920 °F
Softening Point 1700 °C3090 °F
Annealing Point 1220 °C2230 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45851.4585
 
Component Elements PropertiesMetricEnglishComments
SiO2 99.95 %99.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
S-Glass Fiber, Generic
UBE Tyrannohex® Heat Resistant Composite
AGY ZenTron® S-2 Generic S-Glass Fiber
A-Glass Fiber, Generic
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber

CSTGQZ10 / 2228

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.