MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Brush 60™ HT
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Information supplied by Brush Wellman Engineered Materials.

Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%
Stress Relaxation after 1000 hrs @ 200°C: 75%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.5
Formability Ratio (bad Way): 1.5
Superficial Hardness: 30T 82-89

Brush 60™ is a new generation, high conductivity copper beryllium alloy which is specifically engineered to meet the stringent electrical and mechanical requirements of computer, datacom, and telecommunications applications. Performance benefits include:

  • Signal reliability
  • Durability
  • Design flexibility
  • Manufacturability
  • Recyclability

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: UNS C17460
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 99 - 10699 - 106
Tensile Strength, Ultimate 825 - 965 MPa120000 - 140000 psi
Tensile Strength, Yield 720 - 860 MPa104000 - 125000 psi
Elongation at Break >= 10 %>= 10 %
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000340 ohm-cm<= 0.00000340 ohm-cm>5% IACS conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 221 W/m-K1530 BTU-in/hr-ft²-°F
Melting Point 1030 - 1080 °C1890 - 1980 °F
Solidus 1030 °C1890 °F
Liquidus 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.15 - 0.50 %0.15 - 0.50 %
Copper, Cu 98.1 %98.1 %as balance
Nickel, Ni 1.0 - 1.4 %1.0 - 1.4 %
Tin, Sn <= 0.25 %<= 0.25 %
Zirconium, Zr <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brush Wellman Beryllium-Copper Alloy 171 1/4 HT (TH01) Temper
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500)
Materion Beryllium Nickel M220C
Materion Beryllium Nickel Strip - Alloy 360 Annealed

NBB261 / 15118

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.