MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Imerys Hamilton™ Kaolin
Categories: Ceramic; Clay; Kaolin Clay; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel ability.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.50 µm0.50 µm69% finer than
 1.0 µm1.0 µm83% finer than
 2.0 µm2.0 µm89% finer than
 5.0 µm5.0 µm95% finer than
 10 µm10 µm98% finer than
 20 µm20 µm99% finer than
Particle Mesh Size 325 Mesh325 Mesh2% retained
pH 4.04.0
Specific Surface Area 24 m²/g24 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00207 GPa0.300 ksi
 
Component Elements PropertiesMetricEnglishComments
Al2O3 38.8 %38.8 %
CaO 0.20 %0.20 %
Carbon, C 0.030 %0.030 %
Fe2O3 1.3 %1.3 %
K2O 0.20 %0.20 %
Loss on Ignition(%) 14 %
@Temperature 950 °C
14 %
@Temperature 1740 °F
MgO 0.20 %0.20 %
Na2O 0.10 %0.10 %
P2O5 0.10 %0.10 %
SiO2 44 %44 %
Sulfur, S 0.080 %0.080 %
TiO2 1.5 %1.5 %
 
Descriptive Properties
M.B.I. (meq/100g)4.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys ImerPlast™ 20 Recycled Polyolefin for Pipe Extrusion
Imerys KT-Cast/Rogers™ Kaolin
Imerys Kingsley - Rogers™ Kaolin

CIMERY040 / 88390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.